Fast curing
The viscosity of the 1140 resin in use is in the range of 20 to 40 seconds/23°C, and the viscosity of the impregnating resin determines the amount of paint hanging and the fullness of the insulation. If the viscosity is large, the amount of paint is large, and the insulation is plump, which is suitable for large workpieces. If the viscosity is low, the amount of paint hanging is small, and the lacquer distillate is small. It does not need to shovel paint. It is suitable for small or dense winding coils and occasions where paint cannot be shoveled. Due to the good mechanical and electrical properties of 1140 resin, low viscosity impregnation can also obtain good insulation effect. The user can determine the control viscosity of the 1140 resin according to the workpiece type and insulation requirements. The common viscosity range is 25~30 seconds/23 ℃ for No. 4 viscometer.
Classification:
Insulation impregnating varnish series
Keywords:
Fast curing
Details
Method of use
1.1140 resin is mainly used in ordinary immersion and vacuum impregnation insulation process, and is also suitable for use on composite vacuum impregnation dryer. 1140 resin is generally used in a impregnation process, for the use of poor environment, or special requirements have a higher insulation fullness can be used in the second impregnation process.
2. Viscosity and adjustment of impregnating resin
The viscosity of the 1140 resin in use is in the range of 20 to 40 seconds/23°C, and the viscosity of the impregnating resin determines the amount of paint hanging and the fullness of the insulation. If the viscosity is large, the amount of paint is large, and the insulation is plump, which is suitable for large workpieces. If the viscosity is low, the amount of paint hanging is small, and the lacquer distillate is small. It does not need to shovel paint. It is suitable for small or dense winding coils and occasions where paint cannot be shoveled. Due to the good mechanical and electrical properties of 1140 resin, low viscosity impregnation can also obtain good insulation effect. The user can determine the control viscosity of the 1140 resin according to the workpiece type and insulation requirements. The common viscosity range is 25~30 seconds/23 ℃ for No. 4 viscometer.
When the viscosity is higher than the control range, use the 1140-X special diluent to lower. The cumulative amount of 1140-X diluent is generally not more than 35% of the original paint, and when the viscosity is controlled below 23 seconds/23 ℃, the user should order special specifications of 1140 resin from our company.
3. General immersion reference process
3.1 workpiece pre-drying
The pre-drying of the workpiece plays the role of preheating and de-damp, making the workpiece easy to impregnate and stabilizing the insulation quality. The pre-drying temperature and time can be determined according to the structure and size of the workpiece and other factors. The common temperature is 100~130 ℃ for 2~4 hours.
3.2 impregnation
The pre-baked workpiece is naturally cooled to 50~60 ℃ and then immersed in the resin tank. The workpiece should be immersed below 50mm of the liquid level and immersed for 10~20 minutes until no bubbles escape.
3.3 dripping dry
Drop at room temperature for 30-60 minutes until no resin drops, and the dripping time should be long but not short.
3.4 curing
After the workpiece dries, it is pushed into the oven (room) heated to the curing temperature. The curing temperature is generally 125~135 ℃, and the heat preservation is 3~5 hours. If the workpiece is pushed into the cold oven and then heated, the baking time shall be calculated from the time the temperature reaches the curing temperature.
3.5 considerations
(1) When not working, the paint cylinder should be covered in time to avoid volatilization of diluent and mixing of impurities.
(2) The temperature of the workpiece during impregnation should not be too high, and it is advisable to control the temperature of the impregnated resin not to exceed 35°C.
(3) The temperature in the oven should be kept uniform, and the temperature difference between the highest temperature and the lowest temperature should not exceed 10°C,
Otherwise, it may affect the consistency of product quality.
(4) Impregnated resin is inflammable and explosive. Impregnation workshop should pay attention to safe production and no fireworks.
4. Composite vacuum impregnation dryer using reference process
Pre-drying of 4.1: heat up to 50~60 ℃, keep the temperature for 30 minutes, vacuum to above-0.09Mpa, keep for 5 minutes, and then transfer paint.
4.2 vacuum impregnation: close the vacuum valve, transport paint to at least 50mm above the workpiece, close the paint inlet valve, vacuum to the vacuum degree of-0.06Mpa or more for 5 minutes.
4.3 Atmospheric Impregnation: Impregnation at atmospheric pressure for at least 5 minutes.
4.4 paint return: vacuum the paint storage tank to -0.08MPa to complete paint return.
4.5 dripping dry: after dripping paint for 40~60 minutes, vacuum to above-0.08MPa and return the dripping paint.
4.6 cleaning: use a cleaning pump to pump the 1140-x diluent into the bottom of the dipping tank for 5-10 minutes and then pump the diluent back to the diluent storage tank.
4.7 vacuum paint collection: heat up to 60~70 ℃, and vacuum paint collection can be carried out once at 90~100 ℃: stop heating, vacuum to above-0.08MPa and keep for 2~5 minutes. Vacuum paint cleaning can be repeated once after low temperature paint collection.
4.8 curing: generally work at 125~135 ℃ heat preservation for 3~5 hours (note: the temperature reaches 125 ℃ to start timing). Special work according to the actual situation.
4.9 Notes:
(1) When heating, the fan should be turned on for 5 minutes before turning on the electric heater; when the heating is stopped, the electric heater should be cut off for 5 minutes before stopping the fan.
(2) Unless the impregnation system is in a vacuum state, it must be emptied, and the equipment with exhaust fan should turn on the exhaust fan at the same time.
Packaging and storage
The 1140 resin is packed in 18kg or 200kg iron drums. The original packaging is stored in a dry and cool room or under a shelter. The storage period is eight months from the date of delivery.